Uainishaji wa AWS: AWS 5.9
MAELEZO:
Waya za kulehemu za chuma cha pua zina ufanisi mkubwa wa kufunika, utendaji mzuri wa kiufundi wa kulehemu katika kulehemu kwa nafasi zote. Zinatumika sana katika tasnia: muundo wa majengo, gari, uhandisi wa daraja, mashine za madini, reli, bomba la mafuta, vifaa vya kubeba shinikizo la gesi, vifaa vya umeme, n.k.
NAMBA YA MFANO NA UKUBWA:
1. Huduma ya OEM ya kiwandani.
2. Mfano: ER308 ER308L ER308LSi ER309 ER309L ER316 ER316L ER316LSi n.k.
3. Ukubwa wa waya wa MIG: 0.8mm 0.9mm 1.0mm 1.2mm 1.6mm.
4. Ukubwa wa waya wa TIG: 1.6mm 2.0mm 2.4mm 3.2mm 4.0mm.
UTANGULIZI:
Tunatoa aina tofauti za waya za kulehemu za chuma cha pua, ikiwa ni pamoja na waya za kulehemu za Mig solid, waya za kulehemu za Tig fimbo na waya za kulehemu za submerged-arc, zote ni za ubora wa juu na zinauzwa duniani kote.
Isipokuwa 308 na 309, pia tunatoa 304, 321, 347, 316L, 310, 2209, na 201. Pamoja na vipimo maalum kama vile 318L, 904L, 2594, NiCrMo-3, Ni1.
UFUNGASHAJI:
Ufungashaji wa waya wa kulehemu wa Mig (kifurushi cha spool na ngoma)
Kipenyo: 0.8 - 2.0mm
Kifurushi: Kilo 1/kipande, kilo 5/kipande, kilo 15/kipande, kilo 20/kipande, kilo 100/ngoma, kilo 200/ngoma
Ufungashaji wa waya wa kulehemu kwa fimbo ya tig (mrija wa plastiki)
Kipenyo: 1.0 - 5.0mm
Kifurushi: kilo 5/pakiti
Waya ya kulehemu ya arc iliyozama
Kipenyo: 2.5 - 5.0mm
Kifurushi: 20kg/pakiti, 25kg/pakiti
Ufungashaji usio na upande wowote na OEM zinakaribishwa!
MIUNDO YA KIKEMIKALI YA WAYA WA KULEHEMU CHUMA CHAFU:
| Nambari ya Mfano | C | Si | Mn | P | S | Cr | Ni | Mo | Cu |
| 304 | 0.08 | 0.30-1.00 | 2.00 | 0.045 | 0.030 | 18.00-20.00 | 8.00-11.00 | 0.18 | 0.003 |
| 304L | 0.03 | 0.30-1.00 | 2.00 | 0.045 | 0.030 | 18.00-20.00 | 8.00-12.00 | ||
| ER307 | 0.04-0.14 | 0.30-0.65 | 4.30-4.75 | 0.030 | 0.030 | 19.50-22.00 | 8.00-10.70 | 0.5-1.5 | 0.75 |
| ER308 | 0.08 | 0.30-0.65 | 4.30-4.75 | 0.030 | 0.030 | 19.50-22.00 | 9.00-11.00 | 0.75 | 0.75 |
| ER308L | 0.03 | 0.30-0.65 | 1.50-2.30 | 0.03 | 0.02 | 19.5-21.5 | 9.00-11.00 | 0.75 | 0.75 |
| ER308LSi | 0.03 | 0.65-1.00 | 1.60-2.40 | 0.03 | 0.02 | 19.5-21.5 | 9.0-11.0 | 0.75 | 0.75 |
| ER309 | 0.12 | 0.30-0.65 | 1.00-2.50 | 0.03 | 0.03 | 24.0-25.0 | 12.0-14.0 | 0.75 | 0.75 |
| ER309L | 0.03 | 0.3-0.65 | 1.5-2.3 | 0.03 | 0.02 | 23.0-25.0 | 12.0-14.0 | 0.75 | 0.75 |
| ER309LSi | 0.03 | 0.65-1.0 | 1.6-2.4 | 0.03 | 0.02 | 23.0-25.0 | 12.0-14.0 | 0.75 | 0.75 |
| ER316 | 0.08 | 0.3-0.65 | 1.0-2.5 | 0.03 | 0.03 | 18.00-12.00 | 11.0-14.0 | 2.0-3.0 | 0.75 |
| ER316L | 0.03 | 0.3-0.65 | 1.5-2.3 | 0.03 | 0.02 | 18.0-20.0 | 11.0-13.0 | 2.05-2.55 | 0.75 |
| ER316LSi | 0.03 | 0.65-1.0 | 1.6-2.4 | 0.03 | 0.02 | 18.0-20.0 | 11.0-13.0 | 2.05-2.55 | 0.75 |
| ER310 | 0.08-0.15 | 0.3-0.65 | 1.0-2.5 | 0.03 | 0.03 | 25.0-28.0 | 20.0-22.5 | 0.75 | 0.75 |
| ER347 | 0.08 | 0.3-0.65 | 1.0-2.5 | 0.03 | 0.03 | 19.0-21.5 | 9.0-11.0 | 0.75 | 0.75 |
| ER317 | 0.08 | 0.3-0.65 | 1.0-2.5 | 0.03 | 0.01 | 18.5-20.5 | 13.0-15.0 | 3.0-4.0 | 0.75 |
| ER321 | 0.08 | 0.3-0.65 | 1.5-2.5 | 0.03 | 0.01 | 18.5-20.5 | 9.0-10.5 | 0.75 | 0.75 |
| Nambari ya Mfano | Nguvu ya mvutano Rm(Mpa) | Nguvu ya mavuno Rel au Rp0.2(Mpa) | Kurefusha (%) | Nambari ya Mfano | Nguvu ya mvutano Rm(Mpa) | Nguvu ya mavuno Rel au Rp0.2(Mpa) | Kurefusha (%) |
| 304 | 550 | -- | 25 | ER309LSi | 510 | 320 | 25 |
| 304L | 510 | -- | 25 | ER316 | 510 | 320 | 25 |
| ER307 | 590 | 350 | 25 | ER316L | 510 | 320 | 25 |
| ER308 | 550 | 350 | 25 | ER316LSi | 510 | 320 | 20 |
| ER308L | 510 | 320 | 25 | ER310 | 550 | 350 | 25 |
| ER308LSi | 510 | 320 | 25 | ER347 | 550 | 350 | 25 |
| ER309 | 550 | 350 | 25 | ER317 | 550 | 350 | 25 |
| ER309L | 510 | 320 | 25 | ER321 | 550 | 350 | 25 |
| Muundo wa waya wa kulehemu chuma cha pua cha TIG na MIG | ||||||||||
| YB5092-2005 | AWS | Muundo wa Kemikali % | ||||||||
| C | Si | Mn | P | S | Cr | Ni | Mo | |||
| H08Cr20Ni9Mn7Si | ER307Si | 0.075 | 0.78 | 6.7 | 0.022 | 0.01 | 19.8 | 8.8 | ||
| H06Cr21Ni10 | ER308 | 0.045 | 0.45 | 1.9 | 0.02 | 0.009 | 20.8 | 9.8 | ||
| H0OCr21Ni10 | ER308L | 0.02 | 0.32 | 1.9 | 0.011 | 0.006 | 20 | 10.2 | ||
| H06Cr21Ni10Si | ER308Si | 0.045 | 0.85 | 1.5 | 0.022 | 0.01 | 20.8 | 9.8 | ||
| H06Cr24Ni13 | ER309 | 0.06 | 0.45 | 1.9 | 0.019 | 0.009 | 24.3 | 13.2 | ||
| H06Cr24Ni13Si | ER309Si | 0.06 | 0.79 | 1.95 | 0.019 | 0.009 | 24.7 | 13.2 | ||
| H03Cr24Ni13 | ER309L | 0.02 | 0.42 | 1.8 | 0.02 | 0.01 | 24.8 | 13.2 | ||
| H03Cr24Ni13Si | ER309LSi | 0.018 | 0.8 | 1.7 | 0.02 | 0.01 | 23.5 | 13.5 | ||
| H21Cr16Ni35 | ER330 | 0.2 | 0.38 | 1.5 | 0.022 | 0.01 | 16.5 | 34.5 | ||
| H06Cr19Ni12Mo2 | ER316 | 0.04 | 0.4 | 1.9 | 0.02 | 0.01 | 19.5 | 11.8 | 2.3 | |
| H06Cr19Ni12Mo2Si | ER316Si | 0.05 | 0.7 | 1.92 | 0.02 | 0.01 | 19.5 | 11.8 | 2.3 | |
| H03Cr19Ni12Mo2 | ER316L | 0.019 | 0.38 | 1.8 | 0.018 | 0.01 | 19.8 | 12.2 | 2.5 | |
| H03Cr19Ni12Mo2Si | ER316LSi | 0.06 | 0.85 | 1.7 | 0.022 | 0.01 | 18.8 | 12.6 | 2.4 | |
| H03Cr17Ni14Mo3 | ER317L | 0.02 | 0.38 | 1.8 | 0.02 | 0.01 | 18.8 | 13.8 | 3.6 | |
| H08Cr19Ni12Mo2Nb | ER318 | 0.06 | 0.42 | 1.5 | 0.022 | 0.01 | 18.5 | 11.8 | 2.3 | |
| H07Cr20Ni34Mo2Cu3Nb | ER320 | 0.06 | 0.4 | 1 | 0.022 | 0.01 | 19.8 | 33.3 | 2.8 | Nambari 0.7 |
| H02Cr20Ni34Mo2Cu3Nb | ER320L | 0.018 | 0.33 | 1.5 | 0.013 | 0.01 | 19.8 | 33.6 | 2.5 | Nambari 0.35 |
| H08Cr20Ni10Ti | ER321 | 0.06 | 0.45 | 1.5 | 0.022 | 0.01 | 20.8 | 9.8 | Ti9xC-1.0 | |
| H08Cr21 Ni10Nb | ER347 | 0.055 | 0.48 | 1.8 | 0.021 | 0.008 | 20.8 | 9.8 | Nb1xC-1.0 | |
| H12Cr26Ni21 | ER310 | 0.09 | 0.5 | 1.66 | 0.02 | 0.01 | 25.5 | 20.5 | ||
| H02Cr20Ni25Mo4Cu | ER385 | 0.02 | 0.3 | 1.5 | 0.018 | 0.01 | 20.2 | 24.8 | 4.8 | Cu 1.80 |
| H03Cr22Ni9Mo3N | ER2209 | 0.022 | 0.5 | 0.9 | 0.02 | 0.01 | 22.5 | 8.8 | 3.3 | N0.08-0.20 |
| H04Cr25Ni5Mo3Cu2N | ER2553 | 0.027 | 0.5 | 1 | 0.025 | 0.015 | 24.8 | 5.5 | 3.2 | N0.1-0.25 |
| H1 5Cr29Ni9 | ER312 | 0.09 | 0.38 | 1.5 | 0.022 | 0.01 | 29.5 | 8.5 | ||
| H03Cr24Ni13MoL | ER309L Mwezi | 0.023 | 0.45 | 1.5 | 0.022 | 0.01 | 23.8 | 13.2 | 2.2 | |
| H05Cr17Ni4Cu4Nb | ER630 | 0.04 | 0.39 | 0.5 | 0.022 | 0.01 | 16.5 | 4.8 | Cu; Nambari 3; 0.28 | |
| H08Cr26Ni5Mo2 | ER453 | 0.06 | 0.3 | 0.4 | 0.022 | 0.01 | 25.8 | 4.8 | 2.1 | |
| H08Cr21Ni10Mn6 | 0.06 | 0.35 | 5.5 | 0.022 | 0.01 | 20.8 | 9.8 | |||
| H05Cr22Ni11Mn6Mo3VN | ER209 | 0.04 | 0.4 | 4.5 | 0.022 | 0.01 | 21.5 | 10.8 | 2.2 | N;0.20 V;0.18 |
Wenzhou Tianyu Electronic Co., Ltd. ilianzishwa mwaka wa 2000. Tumekuwa tukijishughulisha na utengenezaji wa elektrodi za kulehemu, fimbo za kulehemu, na vifaa vya kulehemu kwa zaidi ya miaka 20.
Bidhaa zetu kuu ni pamoja na elektrodi za kulehemu za chuma cha pua, elektrodi za kulehemu za chuma cha kaboni, elektrodi za kulehemu za aloi ya chini, elektrodi za kulehemu za uso, elektrodi za kulehemu za aloi ya nikeli na kobalti, waya za kulehemu za chuma laini na aloi ya chini, waya za kulehemu za chuma cha pua, waya zenye mgandamizo wa mtiririko unaolindwa na gesi, waya za kulehemu za alumini, waya za kulehemu za aloi ya nikeli na kobalti zilizozama. waya, waya za kulehemu za aloi ya nikeli na kobalti, waya za kulehemu za shaba, waya za kulehemu za TIG na MIG, elektrodi za tungsten, elektrodi za kuchomea kaboni, na vifaa vingine vya kulehemu na vifaa vya matumizi.
Wenzhou Tianyu Electronic Co., Ltd. ilianzishwa mwaka wa 2000. Tumekuwa tukijishughulisha na utengenezaji wa elektrodi za kulehemu, fimbo za kulehemu, na vifaa vya kulehemu kwa zaidi ya miaka 20.
Bidhaa zetu kuu ni pamoja na elektrodi za kulehemu za chuma cha pua, elektrodi za kulehemu za chuma cha kaboni, elektrodi za kulehemu za aloi ya chini, elektrodi za kulehemu za uso, elektrodi za kulehemu za aloi ya nikeli na kobalti, waya za kulehemu za chuma laini na aloi ya chini, waya za kulehemu za chuma cha pua, waya zenye mgandamizo wa mtiririko unaolindwa na gesi, waya za kulehemu za alumini, waya za kulehemu za aloi ya nikeli na kobalti zilizozama. waya, waya za kulehemu za aloi ya nikeli na kobalti, waya za kulehemu za shaba, waya za kulehemu za TIG na MIG, elektrodi za tungsten, elektrodi za kuchomea kaboni, na vifaa vingine vya kulehemu na vifaa vya matumizi.